Abstract

Production of cement paste cylindrical specimens developed for creep tests at variable humidities and/or temperatures is described. The wall thickness is only 0.75 mm, which is required so that an equilibrium humidity distribution can be achieved in a short time with the result that the material parameters may be obtained directly by experiment.

Original languageEnglish (US)
Pages (from-to)277-281
Number of pages5
JournalMatériaux et Constructions
Volume6
Issue number4
DOIs
StatePublished - Jul 1 1973

ASJC Scopus subject areas

  • Engineering(all)

Fingerprint

Dive into the research topics of 'A thin-wall cement paste cylinder for creep tests at variable humidity or temperature'. Together they form a unique fingerprint.