Bloating in (Pb 0.95Sn 0.05Te) 0.92(PbS) 0.08-0.055%PbI 2 thermoelectric specimens as a result of processing conditions

Jennifer E. Ni*, Eldon D. Case, Ryan Stewart, Chun I. Wu, Timothy P. Hogan, Mercouri G. Kanatzidis

*Corresponding author for this work