Nanoscale studies of the chemistry of a René N6 superalloy

Kevin E. Yoon, Dieter Isheim, Ronald D. Noebe, David N. Seidman*

*Corresponding author for this work

Research output: Contribution to journalArticlepeer-review

49 Scopus citations

Fingerprint

Dive into the research topics of 'Nanoscale studies of the chemistry of a René N6 superalloy'. Together they form a unique fingerprint.

Chemical Compounds

Physics & Astronomy

Engineering & Materials Science