Abstract
The size and shape of magnetic chitosan particles were found to be dependent on both the barium ferrite/chitosan (BF/C) ratio and viscosity of a chitosan solution. The saturation magnetization of magnetic chitosan particles varied directly with the BF/C ratio, while coercivity remained almost constant. Notably, incorporated chitosan was shown to exert substantial activity with regard to low cytotoxicity and high heating rate.
Original language | English (US) |
---|---|
Pages (from-to) | 328-333 |
Number of pages | 6 |
Journal | Journal of Magnetism and Magnetic Materials |
Volume | 293 |
Issue number | 1 |
DOIs | |
State | Published - May 1 2005 |
Keywords
- Barium ferrite
- Chitosan
- Coercivity
- Heating rate
- Hyperthermia
- Saturation magnetization
- Toxicity