N2 - A recently developed solution for the plastic strain, ε{lunate}Py(x, t), on the crack line is used in conjunction with a critical strain criterion to construct curves for kR(a) versus a, where a is the increase in crack length. Resistance curves have been computed for various values of the critical plastic strain. They show a monotonic increase of KR(a) with increase in crack length, to a constant steady-state value.
AB - A recently developed solution for the plastic strain, ε{lunate}Py(x, t), on the crack line is used in conjunction with a critical strain criterion to construct curves for kR(a) versus a, where a is the increase in crack length. Resistance curves have been computed for various values of the critical plastic strain. They show a monotonic increase of KR(a) with increase in crack length, to a constant steady-state value.
UR - http://www.scopus.com/inward/record.url?scp=0021975269&partnerID=8YFLogxK
UR - http://www.scopus.com/inward/citedby.url?scp=0021975269&partnerID=8YFLogxK
U2 - 10.1016/0013-7944(85)90045-1
DO - 10.1016/0013-7944(85)90045-1
M3 - Article
AN - SCOPUS:0021975269
VL - 22
SP - 1073
EP - 1078
JO - Engineering Fracture Mechanics
JF - Engineering Fracture Mechanics
SN - 0013-7944
IS - 6
ER -